Loctite® 294 High Temperature/Wicking Grade Threadlocker

Category Polymer , Adhesive , Thermoset
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 294 High Temperature/Wicking Grade Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from delicate electronic components to heavy construction equipment.Loctite® Pre-Applied Threadlockers are dry-to-the-touch films applied to threaded fasteners by fastener suppliers and process centers located throughout North America. Ideally suited for OEMs, they improve speed of assembly and ensure quality by eliminating on-line adhesive dispensing.Loctite® Threadlockers are available in varying viscosities and strengths for virtually any application, including exposure to extreme environments.Loctite® 294 High Temperature/Wicking Grade ThreadlockerIdeally suited for pre-assembled fasteners. Performs well on oily fasteners.Torque capability, M10 steel nuts and bolts: 289 in. lbs. (break), 237 in. lbs. (prevail) Typical Use: High temperature wicking grade
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Viscosity 34.5 cP
34.5 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Full Cure; Steel
Descriptive Properties Value Comments
Color Green