Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Index of Compound 1.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 97
97
ASTM D785
Tensile Strength, Yield 73.5 MPa
10700 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 3.33 GPa
484 ksi
ASTM D790
Izod Impact, Notched 0.157 J/cm
0.294 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
unannealed; ASTM D648
101 °C
214 °F
annealed; ASTM D648
Vicat Softening Point 111 °C
232 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze 0.30 %
0.30 %
ASTM D1003
Transmission, Visible 93 %
93 %
ASTM D1003