Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOTECH® MR 1025 BK Polyamide 66, with mineral filler

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Mineral Filled, Impact Grade
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOTECH®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOTECH® MR 1025 BK Polyamide 66, with mineral filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ISO 1183
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm
0.0060 - 0.012 in/in
Mechanical Properties Metric English Comments
Tensile Stress 110 MPa
16000 psi
Elongation at Yield 2.5 %
2.5 %
Modulus of Elasticity 11.0 GPa
1600 ksi
Flexural Strength 165 MPa
23900 psi
Flexural Modulus 9.00 GPa
1310 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.45
0.45
Coefficient of Friction, Static 0.40
0.40
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
140 °C
284 °F
short term
Vicat Softening Point 240 °C
464 °F
DIN ISO 306
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color black
Users viewing this material also viewed the following: