Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® TPE-7829 Thermoplastic elastomer, with PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
Mechanical Properties Metric English Comments
Tensile Stress 13.0 MPa
1890 psi
Elongation at Yield 1300 %
1300 %
Modulus of Elasticity 0.0400 GPa
5.80 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
110 °C
230 °F
short term
Vicat Softening Point 70.0 °C
158 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 210 °C
410 °F
mass temp
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Zone 1 185 - 205 °C
365 - 401 °F
Zone 2 190 - 210 °C
374 - 410 °F
Zone 3 195 - 215 °C
383 - 419 °F
Mold Temperature 25.0 - 55.0 °C
77.0 - 131 °F
Drying Temperature 85.0 °C

@Time 7200 - 10800 sec
185 °F

@Time 2.00 - 3.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color white