Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
Mechanical Properties Metric English Comments
Tensile Stress 8.00 MPa
1160 psi
Elongation at Yield 500 %
500 %
Modulus of Elasticity 0.200 GPa
29.0 ksi
Charpy Impact, Notched 3.30 J/cm²
15.7 ft-lb/in²
ISO 179 1eA
Electrical Properties Metric English Comments
Insulation Resistance 100 - 100000 ohm
100 - 100000 ohm
Processing Properties Metric English Comments
Processing Temperature 210 °C
410 °F
mass temp
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Zone 1 185 - 205 °C
365 - 401 °F
Zone 2 190 - 210 °C
374 - 410 °F
Zone 3 195 - 215 °C
383 - 419 °F
Mold Temperature 25.0 - 55.0 °C
77.0 - 131 °F
Drying Temperature 85.0 °C

@Time 7200 - 10800 sec
185 °F

@Time 2.00 - 3.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color grey