Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/BK Polyamide 66, with glass fiber and PTFE

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber/PTFE Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/BK Polyamide 66, with glass fiber and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable precision parts with low warpage and narrow tolerance range.Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 150 MPa
21800 psi
Elongation at Yield 3.0 %
3.0 %
4.0 %
4.0 %
flexural
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 220 MPa
31900 psi
Flexural Modulus 7.50 GPa
1090 ksi
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
flatwise; ISO 179 1fU
4.60 J/cm²

@Temperature -30.0 °C
21.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.23
0.23
Coefficient of Friction, Static 0.18
0.18
Thermal Properties Metric English Comments
CTE, linear 25.0 µm/m-°C
13.9 µin/in-°F
DIN 53752
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 100 °C
212 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
Vicat Softening Point 250 °C
482 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color black