Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Carbon Fiber/PTFE Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suitable for continuous discharging of statically generated electricity.Gear parts for automotive appliances, control disks, cams, sliding elements.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 160 MPa
23200 psi
Elongation at Yield 3.0 %
3.0 %
3.5 %
3.5 %
flexural
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 230 MPa
33400 psi
Flexural Modulus 8.00 GPa
1160 ksi
Charpy Impact Unnotched 4.60 J/cm²
21.9 ft-lb/in²
edgewise; ISO 179 1eU
Coefficient of Friction, Dynamic 0.18
0.18
Coefficient of Friction, Static 0.11
0.11
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
DIN 53752
Thermal Conductivity 0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 120 °C
248 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
Vicat Softening Point 250 °C
482 °F
DIN ISO 306
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
Insulation Resistance <= 100000 ohm
<= 100000 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color grey