Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running property.Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.011 - 0.018 cm/cm
0.011 - 0.018 in/in
Mechanical Properties Metric English Comments
Tensile Stress 85.0 MPa
12300 psi
Elongation at Yield 6.0 %
6.0 %
8.5 %
8.5 %
flexural
Modulus of Elasticity 3.50 GPa
508 ksi
Flexural Strength 120 MPa
17400 psi
Flexural Modulus 3.00 GPa
435 ksi
Charpy Impact Unnotched 3.80 J/cm²
18.1 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
160 °C
320 °F
short term
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 310 °C
590 °F
mass temp
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Zone 1 285 - 315 °C
545 - 599 °F
Zone 2 305 - 315 °C
581 - 599 °F
Zone 3 305 - 315 °C
581 - 599 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (yellow)