Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1301-7804 PPS, linear, with carbon fiber, thermally conductive modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Electrically conductive, suitable for continuous discharging of statically generated electricity.Suitable for metall inserts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ISO 1183
Water Absorption <= 0.050 %
<= 0.050 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Stress 105 MPa
15200 psi
Elongation at Yield 0.60 %
0.60 %
0.80 %
0.80 %
flexural
Modulus of Elasticity 25.0 GPa
3630 ksi
Flexural Strength 145 MPa
21000 psi
Flexural Modulus 21.0 GPa
3050 ksi
Charpy Impact Unnotched 1.20 J/cm²
5.71 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Thermal Conductivity 6.00 W/m-K
41.6 BTU-in/hr-ft²-°F
HOT-DISK || 60x60x3 mm
Maximum Service Temperature, Air 220 °C
428 °F
240 °C
464 °F
short term
Electrical Properties Metric English Comments
Surface Resistance <= 100 ohm
<= 100 ohm
Insulation Resistance <= 100 ohm
<= 100 ohm
Processing Properties Metric English Comments
Processing Temperature 330 °C
626 °F
mass temp
Nozzle Temperature 320 - 340 °C
608 - 644 °F
Zone 1 300 - 320 °C
572 - 608 °F
Zone 2 310 - 330 °C
590 - 626 °F
Zone 3 320 - 340 °C
608 - 644 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)