Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Stress 210 MPa
30500 psi
Elongation at Yield 1.6 %
1.6 %
2.1 %
2.1 %
flexural
Modulus of Elasticity 22.0 GPa
3190 ksi
Flexural Strength 300 MPa
43500 psi
Flexural Modulus 19.0 GPa
2760 ksi
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
flatwise; ISO 179 1fU
Coefficient of Friction, Dynamic 0.24
0.24
Coefficient of Friction, Static 0.19
0.19
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
280 °C
536 °F
short term
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Surface Resistance <= 1000 ohm
<= 1000 ohm
Insulation Resistance <= 1000 ohm
<= 1000 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)