Latrobe Nitralloy® 135 Modified VAC-ARC, 1.5 to 3 in Premium Nitriding Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel , Carbon Steel , High Carbon Steel
Manufacturer Latrobe Steel
Trade Name Nitralloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Nitralloy® 135 Modified VAC-ARC, 1.5 to 3 in Premium Nitriding Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NITRALLOY 135 MODIFIED VAC-ARC steel is a low alloy nitriding grade with moderate hardenability. It has been designed to provide a high case hardness and to maintain its core strength during the nitriding cycle. VAC-ARC remelting is employed to provide preferred ingot solidification and superior microcleanliness. Nitralloy 135 Modified Vac-Arc steel is also produced by vacuum induction melting followed by vacuum arc remelting (VIM-VAR).Mechanical Properties are Hardened at 1725°F and quench, tempered at 1200°F and air coolInformation Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Mechanical Properties Metric English Comments
Hardness, Brinell 280 - 340
280 - 340
On Surface
Tensile Strength, Ultimate 862 MPa
125000 psi
Tensile Strength, Yield 620 MPa
89900 psi
Elongation at Break 15 %
15 %
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Aluminum, Al 1.2 %
1.2 %
Carbon, C 0.40 %
0.40 %
Chromium, Cr 1.6 %
1.6 %
Iron, Fe 95.55 %
95.55 %
Manganese, Mn 0.60 %
0.60 %
Molybdenum, Mo 0.35 %
0.35 %
Silicon, Si 0.30 %
0.30 %
Users viewing this material also viewed the following: