Latrobe Marvac 250 VIM-VAR ; 5 in. High Strength Maraging Steel

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel , Maraging Steel
Manufacturer Latrobe Steel
Trade Name Marvac
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Marvac 250 VIM-VAR ; 5 in. High Strength Maraging Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which include a low rate of work hardening, good machinability and weldability, and a very simple heat treatment process. Marvac 250 is produced by vacuum induction melting followed by VAC-ARC remelting. This approach provides superior cleanness and a preferred ingot structure to enhance transverse mechanical properties. Marvac 250 is supplied in the solution annealed condition.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1840 MPa
267000 psi
Tensile Strength, Yield 1725 - 1730 MPa

@Strain 0.200 %
250200 - 251000 psi

@Strain 0.200 %
Elongation at Break 12 - 12.2 %
12 - 12.2 %
Reduction of Area 55 - 56 %
55 - 56 %
Fracture Toughness >= 82.0 MPa-m½
>= 74.6 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 23.0 - 482 °C
6.00 µin/in-°F

@Temperature 73.4 - 900 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.10 %
0.10 %
Carbon, C 0.010 %
0.010 %
Cobalt, Co 7.75 %
7.75 %
Iron, Fe 68.24 %
68.24 %
Manganese, Mn 0.10 %
0.10 %
Molybdenum, Mo 4.8 %
4.8 %
Nickel, Ni 18.5 %
18.5 %
Silicon, Si 0.10 %
0.10 %
Titanium, Ti 0.40 %
0.40 %