Latrobe LSSâ„¢ H10 Hot Work Tool Steel (ASTM H10)

Category Metal , Ferrous Metal , Alloy Steel , Chrome-moly Steel , Tool Steel , Hot Work Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ H10 Hot Work Tool Steel (ASTM H10).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS H10 hot work tool steel is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is very resistant to thermal fatigue cracking (heat checking), and can be water cooled in service. TLS H10 is recommended for difficult hot work tooling applications such as hot punches, die casting dies, forging dies, hot shear blades, hot gripper dies, and extrusion tooling.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.78 g/cc
7.78 g/cc
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 41
41
Air Cooled from 1024°C and Double Tempered; 649°C Temper Temperature
58
58
Air Cooled from 1024°C and Double Tempered; 149°C Temper Temperature
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 90 - 95 %
90 - 95 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 21.0 - 204 °C
6.28 µin/in-°F

@Temperature 69.8 - 399 °F
13.5 µm/m-°C

@Temperature 21.0 - 538 °C
7.50 µin/in-°F

@Temperature 69.8 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.42 %
0.42 %
Chromium, Cr 3.15 %
3.15 %
Iron, Fe 92.38 %
92.38 %
Manganese, Mn 0.55 %
0.55 %
Molybdenum, Mo 2.15 %
2.15 %
Silicon, Si 1.0 %
1.0 %
Vanadium, V 0.35 %
0.35 %
Chemical Properties Metric English Comments
Critical Temperature 830 °C
1530 °F
Ac1
Users viewing this material also viewed the following: