Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Lanxess
Trade Name Durethan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smoke density and toxicity, very good electrical properties,
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 270 °C
12 g/10 min

@Load 11.0 lb,
Temperature 518 °F
Estimated using room temperature density; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 73.0 MPa
10600 psi
Conditioned; ISO 527-1/-2
120 MPa
17400 psi
ISO 527-1/-2
Elongation at Break 1.6 %
1.6 %
ISO 527-1/-2
2.2 %
2.2 %
Conditioned; ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
Conditioned; ISO 527-1/-2
12.1 GPa
1750 ksi
ISO 527-1/-2
Charpy Impact Unnotched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eU
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
16.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 181 °C
358 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.20 mm
V-0

@Thickness 0.0472 in
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Form Pellets
ISO Shortname ISO 1874-PA6,MFR,-060N,(MD+GF)65; ISO 1043-PA GF FR(61)
Processing Injection molding
Region Asia Pacific
Europe
Near East/Africa
North America
South and Central America