Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LTL Color Compounds ColorRxâ„¢ PP1-2005ARX Biocompatible Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRxâ„¢ PP1-2005ARX Biocompatible Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 22.8 °C
1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
ASTM D648
Users viewing this material also viewed the following: