LTL Color Compounds ColorRxâ„¢ PC-1001A Antimicrobial Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRxâ„¢ PC-1001A Antimicrobial Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 10 melt grade of Polycarbonate containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.12 %
0.12 %
@ 24 Hours, 73ºF; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Tensile Strength, Yield 64.1 MPa
9300 psi
ASTM D638
Elongation at Break 112 %
112 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
0.125"; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed (0.250"); ASTM D648