Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LTL Color Compounds ColorRxâ„¢ ABS-0501A Antimicrobial ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRxâ„¢ ABS-0501A Antimicrobial ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high gloss, injection molding grade of ABS containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.6 MPa
6900 psi
ASTM D638
Elongation at Break 26 %
26 %
ASTM D638
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Temperature 22.8 °C
4.00 ft-lb/in

@Temperature 73.0 °F
0.125"; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.9 °C
183 °F
Unannealed (0.5"); ASTM D648
Users viewing this material also viewed the following: