Material Notes:
General purpose polysulfone with excellent clarityAll information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.3 %
1.3 %
@ 24 Hours; ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0020 cm/cm
0.0015 - 0.0020 in/in
0.125; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 82.7 MPa
12000 psi
2.0 in/min; ASTM D638
Elongation at Break 70 %
70 %
2.0 in/min; ASTM D638
Elongation at Yield 10 %
10 %
2.0 in/min; ASTM D638
Flexural Strength 89.6 MPa
13000 psi
2.0 in/min; ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
2.0 in/min; ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 22.8 °C
1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
Unannealed (0.250"); ASTM D648