Material Notes:
Features: Seetec R3400 is a polypropylene-ethylene random copolymer designed for non-transparent injection molding application. SEETEC R3400 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.Applications: General CPP Film and Non-Transparent Injection MoldingCAS No. 9010-79-1Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 84
84
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
50mm/min; ASTM D638
Elongation at Break <= 500 %
<= 500 %
50mm/min; ASTM D638
Flexural Modulus 0.785 GPa
114 ksi
ASTM D760
Izod Impact, Notched 0.490 J/cm

@Temperature 23.0 °C
0.918 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 - 170 °C
266 - 338 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Vicat Softening Point 135 °C

@Load 1.00 kg
275 °F

@Load 2.20 lb
ASTM D1525
Flash Point >= 340 °C
>= 644 °F
Copyright © lookpolymers.com All Rights Reserved