Material Notes:
Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplication: Bottles for detergents, Household and industrial chemical containers.CAS No. 25213-02-9Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.953 - 0.956 g/cc
0.953 - 0.956 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 30 hour
>= 30 hour
F50; ASTM D1693
Melt Flow 0.30 - 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 - 0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.5 MPa
3840 psi
50 mm/min; ASTM D638
Elongation at Break >= 800 %

@Thickness 50.0 mm
>= 800 %

@Thickness 1.97 in
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Unnotched >= 1.96 J/cm

@Temperature 23.0 °C
>= 3.67 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 132 °C
270 °F
10°C/min; ASTM D3418
Vicat Softening Point 124 °C
255 °F
ASTM D1525