Material Notes:
Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.918 - 0.922 g/cc
0.918 - 0.922 g/cc
ASTM D1505
Melt Flow 2.7 - 3.3 g/10 min

@Load 2.61 kg,
Temperature 190 °C
2.7 - 3.3 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.3 MPa
1780 psi
500mm/min; ASTM D638
Film Elongation at Break, MD 300 %
300 %
500 mm/min; ASTM D638
Film Elongation at Break, TD 550 %
550 %
500 mm/min; ASTM D638
Elongation at Break 600 %
600 %
500 mm/min; ASTM D638
2% Secant Modulus 1.10 GPa
160 ksi
500mm/min; ASTM D638
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
Dart Drop Test 60.0 g
0.132 lb
ASTM D1709
Film Tensile Strength at Break, MD 25.5 MPa
3700 psi
500mm/min, Ultimate; ASTM D638
Film Tensile Strength at Break, TD 22.5 MPa
3260 psi
500mm/min, Ultimate; ASTM D638
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
10°C/min; ASTM D3418
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 95 %
95 %
45°; ASTM D2457