LG Chemical R320 EPS, Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical R320 EPS, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information provided by LG Chemical
Physical Properties Metric English Comments
Water Absorption 0.65 %
0.65 %
[g/100cm<sup>2</sup>], 25g/L; KS M 3808
0.65 %
0.65 %
[g/100cm<sup>2</sup>], 30g/L; KS M 3808
0.80 %
0.80 %
[g/100cm<sup>2</sup>], 20g/L; KS M 3808
1.0 %
1.0 %
[g/100cm<sup>2</sup>], 15g/L; KS M 3808
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.172 MPa
24.9 psi
15g/L; KS M 3808
0.240 MPa
34.8 psi
20g/L; KS M 3808
0.309 MPa
44.8 psi
25g/L; KS M 3808
0.374 MPa
54.2 psi
30g/L; KS M 3808
Impact 0.85
0.85
[kg/cm<sup>2<sup>], 15g/L; KS M 3808
1.23
1.23
[kg/cm<sup>2<sup>], 20g/L; KS M 3808
1.64
1.64
[kg/cm<sup>2<sup>], 25g/L; KS M 3808
2.09
2.09
[kg/cm<sup>2<sup>], 30g/L; KS M 3808
Thermal Properties Metric English Comments
Thermal Conductivity 0.0349 W/m-K
0.242 BTU-in/hr-ft²-°F
30g/L; KS M 3808
0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
25g/L; KS M 3808
0.0384 W/m-K
0.266 BTU-in/hr-ft²-°F
20g/L; KS M 3808
0.0418 W/m-K
0.290 BTU-in/hr-ft²-°F
15g/L; KS M 3808