Material Notes:
Physical Properties: Highly reactive in polymerization and addition reaction. and Colorless, Narcotic gasStructure & Characteristics: Structure and characteristics: CH2=CH-CH3. A colorless inflammable liquefied gas which has characteristic odor of hydrocarbonUses: Film, Plastic, Product, PP resin, Urethane resin, Surfactant, Allyl alcohol, Glycerin epoxy resin, Agricultural medicine, Antioxidant, Plastics, Acetone, Solvent, Paint, Glycerin, Epoxy resinCAS: 115-07-1Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.510 g/cc
0.510 g/cc
Vapor Pressure 9.41 bar

@Temperature 20.0 °C
7060 torr

@Temperature 68.0 °F
Vapor Density=1.48
Thermal Properties Metric English Comments
Boiling Point -48.0 °C
-54.4 °F
Flash Point -108 °C
-162 °F
Descriptive Properties Value Comments
Autoignition Temperature 455°C
Components BUTENE + BD + CYCLOPROPANE + BUTANE
<5 ppm
C2 & LIGHTER
<100 ppm
CO
<5 ppm
CO2
<5 ppm
H2O
<5 ppm
MA & PD
<5 ppm
METHANO
<10 ppm
O2
<5 ppm
PROPANE
<0.4%
PROPYLENE
>99.9%
SULFUR
<2 ppm, as H2S