LG Chemical LUTENE XL8080TR PE Compound

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer LG Chemical
Trade Name LUTENE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUTENE XL8080TR PE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: LUTENE XL8080TR has excellent electrical properties for medium and high voltage power cable insulation and especially it shows improved water tree resistance and has thermal aging property.Applications: Medium and high voltage power cable insulation. (Water Tree Retardant Power Cable Insulation)CAS No: 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.921 g/cc
0.921 g/cc
ISO 1183-D
Degree of Crosslinking >= 80 %
>= 80 %
ASTM D2765A
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 17.65 MPa
>= 2560 psi
ISO 527
>= 16.76 MPa

@Temperature 135 °C,
Time 605000 sec
>= 2431 psi

@Temperature 275 °F,
Time 168 hour
IEC 60811-1-2
Elongation at Break 500 %
500 %
ISO 527
475 %

@Temperature 135 °C,
Time 605000 sec
475 %

@Temperature 275 °F,
Time 168 hour
IEC 60811-1-2
Thermal Properties Metric English Comments
Melting Point 125 - 135 °C
257 - 275 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Dielectric Constant 2.25

@Frequency 1.00e+6 Hz
2.25

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength >= 22.0 kV/mm
>= 559 kV/in
IEC 60243
Dissipation Factor 0.00060

@Frequency 1.00e+6 Hz
0.00060

@Frequency 1.00e+6 Hz
IEC 60250