LG Chemical Acetone

Category Fluid
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical Acetone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: Acetone is the raw material of MMA(Methyl Metha Acrylate), BPA, ascorbic acid (Vitamin C), etc. In addition, acetone is widely used as solvents for synthetic resins, rubber, oil paper and paints, as well as for acetyl cellulose, nitro cellulose, etc. By applying the cumene process, LG Petrochemical produces acetone and phenol by using benzene and propylene as raw materials. Acetone is a colorless liquid with a distinct smell and is inflammable due to its low boiling point. CAS: 67-64-1Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.791 - 0.793 g/cc
0.791 - 0.793 g/cc
Viscosity 0.256 cP

@Temperature 50.0 °C
0.256 cP

@Temperature 122 °F
0.33 cP

@Temperature 20.0 °C
0.33 cP

@Temperature 68.0 °F
Dynamic
0.331 cP

@Temperature 20.0 °C
0.331 cP

@Temperature 68.0 °F
0.401 cP

@Temperature 0.000 °C
0.401 cP

@Temperature 32.0 °F
Molecular Weight 58.08 g/mol
58.08 g/mol
Vapor Pressure 0.0923 bar

@Temperature 0.000 °C
69.2 torr

@Temperature 32.0 °F
0.241 bar

@Temperature 20.0 °C
181 torr

@Temperature 68.0 °F
0.3766 bar

@Temperature 30.0 °C
282.5 torr

@Temperature 86.0 °F
0.5606 bar

@Temperature 40.0 °C
420.5 torr

@Temperature 104 °F
Surface Tension 22.8 dynes/cm
22.8 dynes/cm
Thermal Properties Metric English Comments
Heat of Fusion 96.0 J/g
41.3 BTU/lb
Heat of Vaporization 512000 J/g

@Temperature 56.1 °C
220000 BTU/lb

@Temperature 133 °F
CTE, linear 0.00140 µm/m-°C
0.000778 µin/in-°F
Thermal Conductivity 0.160 W/m-K
1.11 BTU-in/hr-ft²-°F
Melting Point -95.35 °C
-139.6 °F
Boiling Point 56.2 °C
133 °F
Flash Point -20.0 °C
-4.00 °F
TOC
-9.00 °C
15.8 °F
CC
Optical Properties Metric English Comments
Refractive Index 1.359
1.359
Electrical Properties Metric English Comments
Dielectric Constant 21.4
21.4
Descriptive Properties Value Comments
Acidity <20 ppm
Autoignition Temperature ASTM D2155
Color <5 Pt/Co
Clear liquid
Components Nonvolatiles
<10 ppm
water
<3000 ppm
Explosion limit 2.15-13%
25°C
Heat of Combustion 7362 cal/g
Ignition Point 456°C
Permanganate Test 150 minutes
Purity >99.7%
Total Distillation Range <0.8°C