Material Notes:
High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superior extrusion processing suitable for OPS, PSP and synthetic wood, Applications include transparent receptacles for medicines and food, toys, goods, audio tapes, stationery, fans, food receptacles, disposable cups, PSP sheet, and film
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 6.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 47.1 MPa
6830 psi
50 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
50 mm/min; ASTM D638
Flexural Yield Strength 91.3 MPa
13200 psi
15 mm/min; ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
15 mm/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 12.7 mm
185 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Flammability, UL94 HB
HB
1/16 in
HB
HB
1/8 in
Flame Spread 28.0 mm/min

@Thickness 3.17 mm
1.10 in/min

@Thickness 0.125 in
FH3
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified