Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
Linear Mold Shrinkage, Flow 0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
Linear Mold Shrinkage, Transverse 0.017 - 0.020 cm/cm
0.017 - 0.020 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
Elongation at Break >= 100 %
>= 100 %
Elongation at Yield 4.0 %
4.0 %
Tensile Modulus 2.20 GPa
319 ksi
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Vicat Softening Point 180 °C

@Load 5.00 kg
356 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
Surface Resistance 100 ohm
100 ohm
Processing Properties Metric English Comments
Melt Temperature 240 - 250 °C
464 - 482 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 100 - 120 °C
212 - 248 °F
Descriptive Properties Value Comments
Electromagnetic reflection 94 dB
ISO Shrinkage - Pressure 60 MPa