Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latishield 66-13A G/30 PA66, Steel/Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Stainless Steel Filled; EMI Grade
Manufacturer LATI
Trade Name Latishield
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 66-13A G/30 PA66, Steel/Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
Linear Mold Shrinkage, Flow 0.0045 - 0.0060 cm/cm
0.0045 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.010 - 0.0125 cm/cm
0.010 - 0.0125 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 9.40 GPa
1360 ksi
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
Vicat Softening Point 245 °C

@Load 5.00 kg
473 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
Surface Resistance 10 ohm
10 ohm
Processing Properties Metric English Comments
Melt Temperature 275 - 300 °C
527 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 90.0 - 100 °C
194 - 212 °F
Descriptive Properties Value Comments
Electromagnetic reflection 93 dB
ISO Shrinkage - Pressure 60 MPa