LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced

Category Polymer , Thermoplastic , ABS Polymer , PC/ABS + Stainless Steel , Polycarbonate (PC)
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 38/11-08A G/10 ABS/PC, Steel/Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on ABS/PC Blend (ABS/PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Linear Mold Shrinkage, Flow 0.0055 - 0.0070 cm/cm
0.0055 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
Elongation at Break 2.2 %
2.2 %
Tensile Modulus 5.50 GPa
798 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
Vicat Softening Point 125 °C

@Load 5.00 kg
257 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 100 ohm
100 ohm
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Drying Temperature 80.0 - 100 °C
176 - 212 °F
Descriptive Properties Value Comments
Electromagnetic reflection 92 dB
ISO Shrinkage - Pressure 60 MPa