Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latigray 66-01 CX/50 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer LATI
Trade Name Latigray
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latigray 66-01 CX/50 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radiopaque compound based on Polyamide 66 (PA66). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm
0.0090 - 0.013 in/in
Linear Mold Shrinkage, Transverse 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 1.6 %
1.6 %
Tensile Modulus 4.80 GPa
696 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Electrical Properties Metric English Comments
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 80.0 - 100 °C

@Time 10800 sec
176 - 212 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: