Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latigea B02 H6 Bio-Polymer

Category Polymer , Thermoplastic , Polylactic Acid (PLA) Biopolymer
Manufacturer LATI
Trade Name Latigea
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latigea B02 H6 Bio-Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
Elongation at Break 1.3 %
1.3 %
Tensile Modulus 5.60 GPa
812 ksi
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Vicat Softening Point 115 °C

@Load 5.00 kg
239 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 170 - 190 °C
338 - 374 °F
Mold Temperature 95.0 - 110 °C
203 - 230 °F
Drying Temperature 40.0 - 60.0 °C

@Time 10800 sec
104 - 140 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Copyright © lookpolymers.com All Rights Reserved