LATI Lastane 50 PUR

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer LATI
Trade Name Lastane
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Lastane 50 PUR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyurethane (PUR). Unfilled. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Elongation at Break >= 100 %

@Temperature 23.0 °C
>= 100 %

@Temperature 73.4 °F
Elongation at Yield >= 100 %

@Temperature 23.0 °C
>= 100 %

@Temperature 73.4 °F
Tensile Modulus 0.250 GPa

@Temperature 23.0 °C
36.3 ksi

@Temperature 73.4 °F
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched NB
NB
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa