Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® with ordinary styrenic soft compounds exhibit excellent rebound properties. Formulation (parts by weight): SEPTON® 4055 - 100, HYBRAR® 5127 - 100, Paraffin Oil - 60, Polypropylene - 40Information provided by The Kuraray Group.
Physical Properties Metric English Comments
Melt Index of Compound 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Tensile Strength, Ultimate 13.9 MPa
2020 psi
Elongation at Break 800 %
800 %
Tensile Modulus 0.00140 GPa
0.203 ksi
Rebound 12 %
12 %
Compression Set 17 %
17 %
25°C, 22 hours
59 %
59 %
70°C, 22 hours