Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kuraray HYBRAR® SC1

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® SC1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® with ordinary styrenic soft compounds exhibit excellent rebound properties. Formulation (parts by weight): SEPTON® 4055 - 100, HYBRAR® 5127 - 100, Paraffin Oil - 100, Polypropylene - 40Information provided by The Kuraray Group.
Physical Properties Metric English Comments
Melt Index of Compound 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 51
51
Tensile Strength, Ultimate 10.3 MPa
1490 psi
Elongation at Break 850 %
850 %
Tensile Modulus 0.00100 GPa
0.145 ksi
Rebound 17 %
17 %
Compression Set 15 %
15 %
25°C, 22 hours
Users viewing this material also viewed the following: