Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® with ordinary styrenic soft compounds exhibit excellent rebound properties. Formulation (parts by weight): SEPTON® 4055 - 100, HYBRAR® 5127 - 0, Paraffin Oil - 180, Polypropylene - 50Information provided by The Kuraray Group.
Physical Properties Metric English Comments
Melt Index of Compound 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 48
48
Tensile Strength, Ultimate 9.30 MPa
1350 psi
Elongation at Break 990 %
990 %
Tensile Modulus 0.000300 GPa
0.0435 ksi
Rebound 40 %
40 %
Compression Set 41 %
41 %
70°C, 22 hours