Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.A low rebound compound can be produced by combining HYBRAR® with an atactic polypropylene and process oil. Formulation (parts by weight): HYBRAR® 5127 - 100, Atactic Polypropylene - 40, Calcium Carbonate - 110, Process Oil - 80, Hydrogenated Petroleum Resin - 150Information provided by The Kuraray Group.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 3.0
3.0
Tensile Strength, Ultimate 0.500 MPa
72.5 psi
Elongation at Break 920 %
920 %
Rebound 16 %
16 %