Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber , Polyethylene (PE) , HDPE
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® and other polymers exhibit excellent vibration damping properties.Mixing Conditions: Brabender Plasticorder @ 200°CMolding Conditions: Press Molding @ 210°C Formulation (parts by weight): High Density Polyethylene - 90, HYBRAR® 5127 - 10Information provided by The Kuraray Group.
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
Tensile Strength, Ultimate 25.0 MPa
3630 psi
Tensile Strength, Yield 47.0 MPa
6820 psi
Elongation at Break 1655 %
1655 %
Tensile Modulus 0.853 GPa
124 ksi
Descriptive Properties Value Comments
Loss Factor 0.077
at 40°C, measured w/ Rheovibron @ 110 Hz
Tan Delta 0.036
measured by resonance method with a cantilever beam
0.07
at 0°C, measured w/ Rheovibron @ 11 Hz
0.072
at 25°C, measured w/ Rheovibron @ 110 Hz