Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kuraray HYBRAR® HD1 Thermoplastic Rubber-HDPE Blend

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber , Polyethylene (PE) , HDPE
Manufacturer Kuraray Company
Trade Name HYBRAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray HYBRAR® HD1 Thermoplastic Rubber-HDPE Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.Blends of HYBRAR® and other polymers exhibit excellent vibration damping properties.Mixing Conditions: Brabender Plasticorder @ 200°CMolding Conditions: Press Molding @ 210°C Formulation (parts by weight): High Density Polyethylene - 80, HYBRAR® 5127 - 20Information provided by The Kuraray Group.
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
Tensile Strength, Ultimate 13.0 MPa
1890 psi
Tensile Strength, Yield 20.0 MPa
2900 psi
Elongation at Break 910 %
910 %
Tensile Modulus 0.343 GPa
49.7 ksi
Descriptive Properties Value Comments
Loss Factor 0.121
at 40°C, measured w/ Rheovibron @ 110 Hz
Tan Delta 0.062
at 0°C, measured w/ Rheovibron @ 11 Hz
0.14
at 25°C, measured w/ Rheovibron @ 110 Hz
0.155
measured by resonance method with a cantilever beam