Kuraray Genestarâ„¢ G1300H Nylon, 30% Glass Filled

Category Polymer , Thermoplastic , Nylon
Manufacturer Kuraray Company
Trade Name Genestar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kuraray Genestarâ„¢ G1300H Nylon, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in a wide range of electrical and electronics components as UL94 HB flammability rating.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
Water Absorption 1.6 %
1.6 %
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 320 °C
45 g/10 min

@Load 4.76 lb,
Temperature 608 °F
ASTM D1238
Spiral Flow 5.30 cm

@Load 750 kg,
Temperature 320 °C
2.09 in

@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
Mechanical Properties Metric English Comments
Tensile Strength 45.0 MPa
6530 psi
Weld; ASTM D638
160 MPa
23200 psi
ASTM D638
Elongation at Yield 0.60 %
0.60 %
Weld; ASTM D638
4.0 %
4.0 %
ASTM D638
Flexural Strength 205 MPa
29700 psi
ASTM D790
Flexural Modulus 8.50 GPa
1230 ksi
ASTM D790
Izod Impact, Notched 1.05 J/cm
1.97 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 306 °C
583 °F
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
ASTM D648
Glass Transition Temp, Tg 125 °C
257 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.3

@Frequency 1.00e+10 Hz
3.3

@Frequency 1.00e+10 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm
762 kV/in
ASTM D149
Dielectric Loss Index 0.0090

@Frequency 1.00e+10 Hz
0.0090

@Frequency 1.00e+10 Hz
ASTM D150
Comparative Tracking Index >= 600 V
>= 600 V
ASTM UL746A