Kraton® G2708 GU (SEBS) Compound

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G2708 GU (SEBS) Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton G2708 GU-N is a formulated compound based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: G2708 GU-N - supplied as a translucent dense pellet.Region: Asia Pacific, Europe, Japan, North America, and South AmericaApplications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; and Impact ModificationInformation provided by Kraton®
Mechanical Properties Metric English Comments
Hardness, Shore A 51 - 61
51 - 61
Injection molded plaque at 205°C; BAM 1003