Kraton® D3158 DT-B (SBS) Compound

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D3158 DT-B (SBS) Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D3158 DT-B is a branched copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified Kraton D3158 DT-B - supplied as a dusted porous pelletRegion: North America, Europe, Asia Pacific, Japan, and South AmericaUses: Kraton D3158 DT-B is used as a modifier of bitumenApplications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.960 - 1.01 g/cc
0.960 - 1.01 g/cc
BAM 1014
Mechanical Properties Metric English Comments
Hardness, Shore A 34 - 44
34 - 44
BAM 1003
Component Elements Properties Metric English Comments
Carbon, C 13.5 - 17.5 %
13.5 - 17.5 %
ASTM D1603
Descriptive Properties Value Comments
Water <1000 ppmw
BAM 1024