Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1192 B (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1192 B (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1192 B is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from South America in the physical form described: Kraton D1192 BT - supplied as a porous pellet dusted with talcRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D1192 B is used for modification of industrial and paving bitumen. It may also be suitable for use in formulating adhesives, sealants and coatings, and in the modification of polymersApplications: Bitumen Modification and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Molecular Weight 138000 - 162000 g/mol
138000 - 162000 g/mol
Triblock
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.10 - 0.40 %
0.10 - 0.40 %
Talc; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 15.0 sec
70

@Time 0.00417 hour
Measured on compression molded slabs; ASTM D2240
Descriptive Properties Value Comments
Content Antioxidant
>0.2%, KM 08
Coupled Polymer
>90%, KM 01
Polystyrene
28.5-32.5%, KM 03
Total Extractables
<1.0%, KM 05
Vinyl
>35%, KM 03
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved