Kraton® D1118 A (SBS) Diblock Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1118 A (SBS) Diblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified: D1118 AT - supplied as porous pellets dusted with talcD1118 AS - supplied as porous pellets dusted with amorphous silicaD1118 ASM - supplied as powder dusted with amorphous silicaRegion: Asia Pacific, Europe, Japan, North America, and South America Uses: Kraton D1118 A is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Volatiles <= 1.0 %
<= 1.0 %
KM 04
Viscosity 470 - 790 cP
470 - 790 cP
25% Toluene Solution at 25°C; KM 06
Ash 0.20 - 0.65 %
0.20 - 0.65 %
AS; ISO 247
0.30 - 0.65 %
0.30 - 0.65 %
AT; ISO 247
2.5 - 5.0 %
2.5 - 5.0 %
ASM; ISO 247
Chemical Properties Metric English Comments
Diblock Content 78 %
78 %
Descriptive Properties Value Comments
Content Antioxidant
0.14-0.36%, KM 08
Polystyrene
31-35%, KM 03
Total Extractables
<1.0%, KM 05