Kraiburg TPE THERMOLAST® K TS6ACZ Black TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TS6ACZ Black TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black compound for applications with reduced requirementsTypical Applications: GripsErasersGrips on stationeriesTransport protectionAnti-slip elementsSkirting boardMaterial Advantages: Excellent price/performance rationAdhesion to PPModerate UV resistanceSmooth surfaceTactile surface (soft touch)Processing: Like polyolefinsHigh injection speed and pressureInformation provided by Kraiburg TPE.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
DIN 53505
Tensile Strength at Break 3.00 MPa
435 psi
DIN 53504
Elongation at Break 460 %
460 %
DIN 53504
Tear Strength 18.0 kN/m
103 pli
DIN 53515
Compression Set 20 %
20 %
72 hours at 23°C; ISO 815
90 %

@Temperature 70.0 °C
90 %

@Temperature 158 °F
24 hours; ISO 815
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Processing Temperature 160 - 200 °C
320 - 392 °F
Descriptive Properties Value Comments
Color Black