Kraiburg TPE THERMOLAST® K TP9HPN Thermoplastic Elastomer, Outdoor Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TP9HPN Thermoplastic Elastomer, Outdoor Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical applications of the EX/UV Series: Edge guardsDistance ProfilesMolded Parts (Solar Equipment)SealsInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
DIN ISO 7619
Tensile Strength 13.0 MPa
1890 psi
DIN 53504/ISO 37
Elongation at Break 700 %
700 %
DIN 53504/ISO 37
Compression Set 29 %

@Temperature 70.0 °C,
Time 86400 sec
29 %

@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
40 %

@Temperature 24.0 °C,
Time 259000 sec
40 %

@Temperature 75.2 °F,
Time 72.0 hour
DIN ISO 815
83 %

@Temperature -25.0 °C,
Time 86400 sec
83 %

@Temperature -13.0 °F,
Time 24.0 hour
DIN ISO 815
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Injection
200 °C
392 °F
Extrusion
Middle Barrel Temperature 180 °C
356 °F
Extrusion
200 °C
392 °F
Injection
Front Barrel Temperature 160 °C
320 °F
Extrusion
220 °C
428 °F
Injection
Die Temperature 190 - 210 °C
374 - 410 °F
Extrusion
Head Temperature 180 °C
356 °F
Extrusion
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Injection
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Extrusion/Injection
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Injection
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Descriptive Properties Value Comments
Color Natural
Hotrunner 200-250°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 230°C
Extrusion
250°C
Injection