Category | Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE |
Manufacturer | |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Kraiburg TPE THERMOLAST® K TP7HPN Natural Extrusion TPE, Outdoor Grade
(Unverified Data**).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 g/cc | 0.0412 lb/in³ | DIN EN ISO 1183-1:2004 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 70 | 70 | DIN 53505/ISO 868 |
Tensile Strength at Break | 10.0 MPa | 1450 psi | Deviating from ISO 37 standard test piece S2 is tested with a traverse speed of 200 mm/min; DIN 53504/ ISO 37 |
Elongation at Break | 750 % | 750 % | Deviating from ISO 37 standard test piece S2 is tested with a traverse speed of 200 mm/min; DIN 53504/ ISO 37 |
Compression Set | 20 % @Temperature 23.0 °C, Time 259000 sec |
20 % @Temperature 73.4 °F, Time 72.0 hour |
ISO 815 |
45 % @Temperature 70.0 °C, Time 79200 sec |
45 % @Temperature 158 °F, Time 22.0 hour |
ISO 815 | |
80 % @Temperature -25.0 °C, Time 79200 sec |
80 % @Temperature -13.0 °F, Time 22.0 hour |
ISO 815 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 160 - 180 °C | 320 - 356 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Color | Natural |