Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraiburg TPE THERMOLAST® K TF7FMA Thermoplastic Elastomer, adhesion to PC, ABS, PETG

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TF7FMA Thermoplastic Elastomer, adhesion to PC, ABS, PETG.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The FC/AD1 Series is recommended for applications with food contact providing excellent adhesion to polar thermoplastics such as PC, ABS and PETG. Typical applications:Function and design elementsGrip applicationsHousehold articlesPackaging (for food and care products) RazorsSealsToothbrushesToysMaterial advantages:Applications with food contactEasy coloring (compounds in natural colors) EN71/3Excellent adhesionExcellent processing behaviorFDA compliantHalogen-freeRegulation (EU) 10/2011Processing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
DIN ISO 7619
Tensile Strength 5.00 MPa
725 psi
DIN 53504/ISO 37
Elongation at Break 550 %
550 %
DIN 53504/ISO 37
Tear Strength 18.0 kN/m
103 pli
DIN ISO 34-1
Peel Strength 10.5 kN/m
59.9 pli
ABS; D41 1916
14.0 kN/m
79.9 pli
PC; D41 1916
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 210 °C
410 °F
Front Barrel Temperature 240 °C
464 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
temperature exceeding 80°C (175°F) should be avoided
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments
Color Natural
Hotrunner 200-205°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 250°C