Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraiburg TPE THERMOLAST® K TF6AAF Thermoplastic Elastomer, Transparent

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TF6AAF Thermoplastic Elastomer, Transparent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The FC/HE/tl Series is recommended for applications with food contact, providing excellent resilience properties. The series is available in translucent colors. Typical applications: Closures Flexible Connections Household articles Membranes Packaging (for food and care products) Seals ValvesMaterial advantages: Applications with food contact Easy coloring (compounds in natural colors) EN71/3 Excellent mechanical properties FDA compliant Halogen-free High resilience Perfect adhesion to PP Regulation (EU) 10/2011 Processing Method: Extrusion, Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 58
58
DIN ISO 7619
Tensile Strength 14.0 MPa
2030 psi
DIN 53504/ISO 37
Elongation at Break 750 %
750 %
DIN 53504/ISO 37
Tear Strength 17.0 kN/m
97.0 pli
DIN ISO 34-1
Compression Set 21 %

@Temperature 25.0 °C,
Time 259000 sec
21 %

@Temperature 77.0 °F,
Time 72.0 hour
DIN ISO 815
32 %

@Temperature 70.0 °C,
Time 86400 sec
32 %

@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
55 %

@Temperature 100 °C,
Time 86400 sec
55 %

@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Injection
200 °C
392 °F
Extrusion
Middle Barrel Temperature 180 °C
356 °F
Extrusion
200 °C
392 °F
Injection
Front Barrel Temperature 160 °C
320 °F
Extrusion
220 °C
428 °F
Injection
Die Temperature 190 - 210 °C
374 - 410 °F
Extrusion
Head Temperature 180 °C
356 °F
Extrusion
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Injection
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Extrusion/Injection
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Injection
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Injection
Descriptive Properties Value Comments
Color Translucent
Hotrunner 200-250°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 230°C
Extrusion
250°C
Injection
Copyright © lookpolymers.com All Rights Reserved