Kraiburg TPE THERMOLAST® K TF4CGN Thermoplastic Elastomer, Natural

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TF4CGN Thermoplastic Elastomer, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The FC Series is a natural-colored and translucent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP.Typical applications:Function and design elementsGrip applicationsHousehold articlesPackaging (for food and care products)RazorsSealsToothbrushesToysMaterial advantages:Adhesion to PPApplications with food contactEasy coloring (compounds in natural colors) EN71/3Excellent mechanical propertiesExcellent processing behaviorFDA compliantHalogen-freeIn natural or translucent availablePleasant surface feel (Soft touch) RecyclableRegulation (EU) 10/2011Processing Method: Injection MoldingInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
DIN EN ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore A 39
39
DIN ISO 7619
Tensile Strength 5.50 MPa
798 psi
DIN 53504/ISO 37
Elongation at Break 850 %
850 %
DIN 53504/ISO 37
Tear Strength 11.0 kN/m
62.8 pli
DIN ISO 34-1
Compression Set 14 %

@Temperature 24.0 °C,
Time 259000 sec
14 %

@Temperature 75.2 °F,
Time 72.0 hour
DIN ISO 815
27 %

@Temperature 70.0 °C,
Time 86400 sec
27 %

@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815
60 %

@Temperature 100 °C,
Time 86400 sec
60 %

@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 200 °C
392 °F
Front Barrel Temperature 220 °C
428 °F
Mold Temperature 25.0 - 40.0 °C
77.0 - 104 °F
Drying Temperature 60.0 - 80.0 °C

@Time 7200 - 14400 sec
140 - 176 °F

@Time 2.00 - 4.00 hour
Injection Pressure 20.0 - 100 MPa
2900 - 14500 psi
Back Pressure 1.97 - 4.90 MPa
285 - 710 psi
Descriptive Properties Value Comments
Color Natural
Hotrunner 200-205°C
The runner should be empty after a maximum of 2 - 3 shots.
Max Cylinder Temperature 250°C