Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraiburg TPE THERMOLAST® K TC9COZ Thermoplastic Elastomer, Automotive interior applications, low density, black

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Kraiburg TPE
Trade Name THERMOLAST® K
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraiburg TPE THERMOLAST® K TC9COZ Thermoplastic Elastomer, Automotive interior applications, low density, black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Markets / Application Sectors:Automotive InteriorAutomotive UndercarApplication Examples:SwitchesSoft grip zonesFile matsCable terminalsMaterial Advantages:Excellent physical propertiesVery good flow characteristicsMeets odor specification for automotive interiorLow densityAdhesion to PPInformation Provided by Kraiburg TPE Corp.
Physical Properties Metric English Comments
Density 0.985 g/cc
0.0356 lb/in³
DIN EN ISO 1183-1:2004
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
DIN 53505 / ISO 868
Tensile Strength at Break 12.2 MPa
1770 psi
Deviating from ISO 37 standard test piece is tested with a traverse speed of 200 mm/min; DIN 53504 / ISO 37
Elongation at Break 670 %
670 %
Deviating from ISO 37 standard test piece is tested with a traverse speed of 200 mm/min; DIN 53504 / ISO 37
Graves Tear Strength 35.0 kN/m
200 pli
DIN ISO 34-1 Method B (b)
Compression Set 43 %

@Temperature 23.0 °C,
Time 259000 sec
43 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
62 %

@Temperature 70.0 °C,
Time 79200 sec
62 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
82 %

@Temperature 100 °C,
Time 79200 sec
82 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Processing Temperature 180 - 250 °C
356 - 482 °F
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved